STB PDF
Specification for nickel-chromium-titanium heat-resisting alloy billets, bars, forgings and parts (nickel base, Cr 19.5, Ti 0.4). Original standard BS 2HR 5-2010 in PDF full version. Additional info + preview on request
Document status: Active
Specification for high expansion heat-resisting steel billets, bars, forgings and parts (Ni 25.5, Cr 15, Ti 2, Mn 1.5, Mo 1.25, Si 0.7, V 0.3) (Solution treated at 980 °C). Original standard BS 2HR 51-2010 in PDF full version. Additional info + preview on request
Document status: Active
Specification for heat-resisting steel billets, bars, forgings and parts (Ni 25.5, Cr 14.7, Ti 1.8, Mn 1.5, Mo 1.2, V 0.3). Original standard BS 2HR 52-2010 in PDF full version. Additional info + preview on request
Document status: Active
Specification for nickel-iron-chromium-molybdenum-titanium heat-resisting alloy billets, bars, forgings and parts (Ni/Co 42.5, Cr 12.5, Mo 5.8, Ti 3.0, Fe remainder). Original standard BS 2HR 53-2010 in PDF full version. Additional info + preview on request
Document status: Active
Specification for nickel-iron-chromium-molybdenum-aluminium-titanium heat-resisting alloy billets, bars, forgings and parts (Ni/Co 43.5, Cr 16.5, Mo 3.3, Al 1.2, Ti 1.2, Fe remainder). Original standard BS 2HR 55-2010 in PDF full version. Additional info + preview on request
Document status: Active
Specification for nickel-chromium- iron-molybdenum-cobalt-tungsten heat-resisting alloy billets, bars, forgings and parts (nickel base, Cr 21.7, Fe 18.5, Mo 9, Co 1.5, W 0.6). Original standard BS 2HR 6-2010 in PDF full version. Additional info + preview on request
Document status: Active