Turkmenistan standards PDF
Alloy Bars and Forgings, Corrosion and Heat Resistant, 38fe 13.2cr 38ni 5.5mo 0.85cb 2.5ti 1.6al 0.009b, Consumable Electrode Melted, Solution and Precipitation Heat Treated. Original standard SAE AMS5634C-1993 in PDF full version. Additional info + preview on request
Document status: Active
Steel, Corrosion-Resistant, Bars, Wire, Forgings and Forging Stock 18Cr - 9Ni - 0.21Pb (303Pb) Free-Machining, Solution Heat Treated. Original standard SAE AMS5635H-2023 in PDF full version. Additional info + preview on request
Document status: Active
Steel, Corrosion-Resistant, Bars and Wire 18Cr - 9.0Ni (302) Solution Heat Treated and Cold Drawn 100 ksi (689 MPa) Tensile Strength. Original standard SAE AMS5636H-2023 in PDF full version. Additional info + preview on request
Document status: Active
Steel, Corrosion-Resistant, Bars and Wire 18Cr - 9.0Ni (302) Solution Heat Treated, Cold Drawn and Stress Relieved 125 ksi (862 MPa) Tensile Strength. Original standard SAE AMS5637K-2023 in PDF full version. Additional info + preview on request
Document status: Active
Steel, Corrosion-Resistant, Bars and Forgings 0.14S - 18Cr - 9.5Ni - 0.50Mo - 0.80Al (303MA) Free-Machining; Swaging or Upsetting Solution Heat Treated. Original standard SAE AMS5638G-2021 in PDF full version. Additional info + preview on request
Document status: Replaced by St SAE AMS5638H-2025
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings and Forging and Ring Stock 19Cr - 10Ni Solution Heat Treated. Original standard SAE AMS5639K-2022 in PDF full version. Additional info + preview on request
Document status: Active