TDS PDF
Iron Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 29Fe - 22Cr - 21Ni - 18.5Co - 3.2Mo - 2.8W - 0.78Ta - 0.30Al - 0.05La - 0.20N Solution Heat Treated. Original standard SAE AMS 5877B-2018 in PDF full version. Additional info + preview on request
Document status: Replaced by St SAE AMS5877C-2023
Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 59Ni - 22Cr - 2Mo - 14W - 0.35Al - 0.03La Solution Heat Treated. Original standard SAE AMS 5878D-2015 in PDF full version. Additional info + preview on request
Document status: Replaced by St SAE AMS5878F-2025
Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Foil 62Ni - 21.5Cr - 9.0Mo - 3.7Cb (Nb) Cold Rolled and Annealed. Original standard SAE AMS 5879D-2015 in PDF full version. Additional info + preview on request
Document status: Replaced by St SAE AMS5879F-2026
Steel, Corrosion-Resistant, Bars, Wire, and Forgings 17Cr 0.52Mo (0.95 1.20C) (SAE 51440C) for Bearing Applications. Original standard SAE AMS 5880E-2013 in PDF full version. Additional info + preview on request
Document status: Replaced by St SAE AMS5880F-2024
Iron-Nickel Alloy, Bars, Forgings, and Rings 42Fe - 37.5Ni - 14Co - 4.8Cb(Nb) - 1.6Ti Solution Heat Treated, Precipitation Hardenable Multiple Melted, High Temperature, Low Expansion. Original standard SAE AMS 5884D-2016 in PDF full version. Additional info + preview on request
Document status: Replaced by St SAE AMS5884E-2022
Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 50Ni - 20Cr - 20Co - 5.8Mo - 2.2Ti - 0.45Al Consumable Electrode or Vacuum Induction Melted 2100 °F (1149 °C) Solution Heat Treated. Original standard SAE AMS 5886C-2014 in PDF full version. Additional info + preview on request
Document status: Replaced by St SAE AMS5886E-2026